Extrusion Processing Guide: TPE – Thermoplastic Elastomers

2019
 Processing Guide: TPE – Thermoplastic Elastomers
 Extruder: Single screw extruder with vacuum
pressure-relieved grooved feeding section (by increased screw pitch and channel depth)
 Screw Design: Barrier screw, 25 – 30 L/D
 Compression Ratio: 3,5:1
 Cylinder Temperatures: 150-185°C
302-365°F
 Melt Temperature: 175-200°C
347-392°F
 Pre-Drying: no,
but 2 hours at 80°C (176°F) if extreme temperature change
 Calibration: no,
but supporting inner pressure if hollow profiles
 Miscellaneous: Breaker plate/screens for higher back pressure and therefore smoother profile surface

Note: This is meant as a general guide. Please consult your material and machinery representative.

Best Deals on TPE Pellets

(check reviews and prices at Ebay)

MultiFLex TPE A 3810 Black plastic Pellets Resin Thermoplastic Elastomer 10 LB
- click here -
1 lb. Dexco Vector SBC  clear plastic Pellets TPE Thermoplastic Elastomer
- click here -
Dexco SBC Vector 4113A plastic clear Pellets TPE Thermoplastic Elastomer 5 LB+
- click here -

Back to PROCESSING GUIDE overview



Related Articles & Comments

Comments are closed.

Latest News

Tweets by @plastics_online