Processing Guide: |
PC – Polycarbonate |
|
Extruder: |
Single screw (profile, sheet, film ) without vacuum, plain feeding section with vacuum or pressure-relieved grooved feeding section (by increased screw pitch and channel depth)
|
|
Screw Design: |
Three-zone screw 25 – 30 L/D or barrier screw |
|
Compression Ratio: |
2,25:1 |
|
Cylinder Temperatures: |
270-300°C
518-572°F
|
|
Melt Temperature: |
290-320°C
554-608°F
|
|
Pre-Drying: |
2-4 hours at 100-120° C (212-248° F) |
|
Calibration: |
|
|
Miscellaneous: |
should not succeed 400°C
reduced wear by preheating of material at 120 C (248 F) or by heating of feeding section at 170 C (338 F)
|
|
Note: This is meant as a general guide. Please consult your material and machinery representative.
– Back to PROCESSING GUIDE overview –