Extrusion Processing Guide: PE-HD – High-density polyethylene

7281
i GET IT
 Processing Guide: PE-HD – High-density polyethylene
 Extruder: Single Screw Extruder with vacuum, grooved feeding section
 Screw Design: Barrier Screw, 25-30 L/D
 Compression Ratio: 3:1
 Cylinder Temperatures: 180-205°C
356-401°F
 Melt Temperature: 180-205°C
356-401°F
 Pre-Drying: No,
3 hours at 105-110°C (221-230°F) for regrind
 Calibration:  
 Miscellaneous: bimodal PE-HD needs motor with 10-15% higher torque and has higher melt pressure/melt temperature
Larger screw diameter : continuously two channels (improved conveying in feeding section)

Note: This is meant as a general guide. Please consult your material and machinery representative.

 